Perma-Chink
Permanantly Distinguish Your Log Home
Add distinctive beauty to your chink-style log home with Perma-Chink, the original synthetic chinking. Its presence on tens of thousands of log structures around the world attests to its lasting appearance and durability.
Superior bonding and flexibility allows Perma-Chink to stretch and maintain a tight seal by following the movement of your logs. Although it looks and feels like traditional mortar, its premium acrylic latex formula will not crack, chip, shrink or fall out. There's simply no better way to seal and protect your chink-style log home.
• Highly Elastic
• Seals 1"-6" Gaps
• Virtually Maintenance-Free
• 5-Year Warranty
Free color swatches are available upon request. Contact one of our Locations.
|
Perma-Chink Specifications
Shelf Life |
|
Application Temperature |
|
Application Methods |
- Chink Pump
- Caulking Gun
- Applicator Bag
|
Surface Preparation |
- Clean and dry
- Backing Material
- Bond-breaker tape on bare wood
|
Frequency |
|
Drying Time |
- Skins over in 1-3 hours
- Cures in 2-8 weeks depending on temperature and
humidity
|
Special Instructions |
- Apply 1/4' - 3/8" thickness
- Avoid applying
in direct sunlight
- Joint should be 1/6th of log diameter
|
To view and/or print MSDS sheets or labels you need Acrobat Reader. If you don't have Acrobat Reader installed on your computer,
click here
for a free download.
| Coverage Rate per Pail |
1/2" Joint |
Use Energy Seal |
3/4" Joint |
Use Energy Seal |
1" Joint |
385 lineal feet |
2" Joint |
192 lineal feet |
3" Joint |
127 lineal feet |
4" Joint |
96 lineal feet |
| 5" Joint |
85 lineal feet |
6" Joint |
63 lineal feet |
|
Perma-chink Application Instructions
(Printer Friendly Version Here)
Application Tips
- Do not apply over freshly applied oil-based stains.
- Practice on the least visible area of the home.
- Use quality tools and caulk guns.
Directions for Use
STEP #1: INSPECTION
If applying to an older home, check for signs of rot and decay. Remove and
replace or repair deteriorated wood. Contact any Perma-Chink Systems office for
information about wood repairs.
STEP #2: SURFACE PREPARATION
All surfaces should be clean, dry and free from oil, dirt or other foreign
matter. Use appropriate materials to clean and prepare surfaces. Perma-Chink Log
Home Sealant is best applied after the home has been stained. We strongly
recommend the use of any LIFELINE™ brand exterior stain and topcoat. If an
oil-based stain has been applied, allow it to dry at least two weeks before
applying Perma-Chink Log Home Sealant.
STEP #3: BACKING MATERIALS
Perma-Chink Log Home Sealant should only be applied over approved substrates.
When selecting the width of Grip Strip to use on round logs, the joint width
should be approximately 1/6th the diameter of the logs (10” diameter logs; 10” ÷
6 = 1.67”). Obtain a copy of our “Log Home Sealant Application Guide” from any
Perma-Chink Systems location for information about suitable backing materials
and substrates.
STEP #4: APPLICATION
Do not apply in direct sunlight or when the temperature is less than 40° F.
Perma-Chink Log Home Sealant may be applied with a bulk loading caulk gun, grout
bag or high volume chink pump. Hold the applicator tip firmly against the back
surface and apply. If several beads of chinking are required to fill a gap,
place them close together to avoid entrapped air. Apply enough sealant to
maintain a wet thickness of at least 5/16” and no more than ½” across the entire
joint after tooling. Only apply as much sealant as you can tool in about 15
minutes. Once the joint is filled, spray with a light mist of water and tool
smooth with a trowel or spatula. If the width of the trowel is close to the
width of the joint, the smoothing process will be easier. Make sure there is
good contact between the Perma-Chink and the exposed edges of the top and bottom
logs. If you are a first time applicator, start work on a less visible area
until you become familiar with the process.
STEP #5: DRYING AND CURING TIME
Protect freshly applied Perma-Chink from direct rainfall for a minimum of 24
hours. When draping a wall with plastic film, allow some airspace between the
wall and the plastic to facilitate drying. Sheets of cardboard may also be use
to cover newly applied Perma-Chink to prevent “chinking inspectors” from leaving
finger dents in the uncured chinking.
Drying time and curing time are two entirely different terms. In warm or hot
weather, Perma-Chink will begin to skin over in as little as ten minutes while a
complete cure may take three to four weeks. Cooler weather will slow both the
drying time and curing process.
STEP #6: CLEANUP
Clean area and equipment immediately with warm, soapy water before the
Perma-Chink dries. For removing Perma-Chink that has dried, soften with alcohol
and then clean with warm water. Please do not pollute our environment. Dispose
of containers and unused material in accordance with local, state, and federal
regulations.
STEP #7: MAINTENANCE
Periodic cleaning with an appropriate cleaner such as Log Wash™ will clean off
dust and dirt and accentuate the beauty of your home. We recommend that log
walls be washed down at least twice a year. Small rips and tears may be repaired
using a bead of Perma-Chink and a damp short bristled brush to blend it in with
the surrounding area. Tears greater than one foot long should be cut out and the
chinking replaced.
STEP #8: STORAGE
Store Perma-Chink out of direct sunlight and protect from freezing. Although
Perma-Chink is freeze-thaw stable, if the product is accidentally frozen, allow
to thaw, mix well and check for suitability of use before applying.